Academic Jobs - Home of Higher Ed Logo

Research spotlight: Thwe Thwe Win on graphene quantum dots that make concrete stronger and harder to corrode

9 min read0 views

At a glance

Graphene quantum dots at 0.1% by weight of cement raised 28-day concrete strength by up to 32% and cut mesopore volume 43%, according to ACS Omega research led by Thwe Thwe Win, now at the University of Lisbon.

a pile of blueberries
Photo by Jack Vaughan on Unsplash

For every tonne of cement in the mix, they added one kilogram of graphene quantum dots. A 0.1% dose by weight of cement. At 28 days, the weakest concrete in their test programme — a 24 MPa mix, the sort poured into pavements and low-rise frames — came out at 37.8 MPa against 28.6 MPa for the identical mix without the dots. That's a 32% lift from an additive measured in parts per ten thousand.

The strength gain is the headline. The mechanism is the story. Thwe Thwe Win, now at the University of Lisbon, and four co-authors show in ACS Omega that the dots did not behave like a filler plugging holes in hardened paste. They changed which hydrate phases formed, and when. The authors put it plainly: the improvement “is not solely associated with a filler effect, but also with hydration-pathway modulation and microstructural refinement induced by GQDs.”

Why this lands now has little to do with strength records. Concrete's carbon bill is paid at the mixer: cement production accounts for roughly 8% of global CO₂ emissions, and the figure keeps being restated because the industry has no fast route to zero. The lever that doesn't require new kilns is service life. A bridge deck that survives 60 years in an acid-bearing sewer instead of 40 spreads the same emissions across half again as many years of use. Win's paper is a durability paper wearing a strength paper's clothes.

Sixteen mixes, four strength grades, three dosages

The team cast ordinary Portland cement concrete at four target strength classes — 24, 28, 32 and 42 MPa — and varied only the additive. Liquid graphene quantum dots went in at 0.1% and 0.3% by weight of cement; a powdered version, which the paper describes as containing a suprastructure of assembled dots, went in at 0.05%. Sixteen mixtures in total, all with the same total water volume and a polycarboxylate superplasticiser.

Graphene quantum dots are flakes of graphene — a sheet of carbon one atom thick — cut so small, under roughly 20 nanometres across, that their edges and surface chemistry dominate their behaviour. They are zero-dimensional in the sense materials scientists use: too small to act as a sheet, too chemically busy to be inert. Their surfaces carry hydroxyl and carboxyl groups, and those groups are what the rest of the paper hangs on.

Testing covered the standard mechanical trio (compressive, splitting tensile, flexural), then water absorption, porosity, and compressive strength retained after 28 and 56 days submerged in acid solution. Splitting tensile strength is the measure of how hard it is to crack a cylinder by loading it sideways, and it usually tracks with how well the paste grips the aggregate. Four instruments then probed the hardened paste: BET nitrogen isotherm analysis for pore surface area and volume, thermogravimetric analysis for how much calcium hydroxide remained, X-ray diffraction for crystalline phases, and field-emission scanning electron microscopy with elemental mapping for what the microstructure actually looked like.

The 43% that matters more than the 32%

Surface area and pore volume tell you whether an additive is filling space or reorganising it. A pure filler can only reduce both by occupying volume. Something that redirects chemistry should leave a different signature.

Strength class28-day compressive, control (MPa)With 0.1% liquid GQDs (MPa)Change
24 MPa28.637.8+32%
28 MPa32.140.7+27%
32 MPa34.637.1+7%
42 MPa44.547.1+6%

The BET numbers came back 16.82 m²/g of surface area and 0.051 cm³/g of pore volume for the control paste. With 0.1% liquid dots: 9.54 m²/g and 0.029 cm³/g. That is a 43% cut in mesopore volume — the pores between roughly 10 and 50 nanometres, the size range that governs how easily water and dissolved sulphate find a way in. Similar doses of graphene oxide and graphene nanoplatelets have typically returned 10–17% strength gains in earlier work, and those materials tend to clump at higher loadings.

Water absorption fell from 6.0% to 4.5% in the 24 MPa class, about a quarter. Porosity in the same mix dropped from 15.9% to 10.8%, roughly a third. The 42 MPa mix only gained 16% on absorption, which the authors attribute to it already being dense — there is less sloppy microstructure left to fix.

A group of blocks of cement stacked together

Photo by Nick Design on Unsplash

What the dots are doing instead of filling holes

Here is the analogy that holds up: imagine a bricklayer working with mortar that sets far too slowly, leaving gaps where bricks haven't yet bonded. Adding sand fills some gaps but slows nothing. Adding a foreman who hands out assignments and keeps the mortar coming changes the finished wall.

The dots act as the foreman. Their oxygen-bearing functional groups attract the clinker minerals that drive setting — alite, belite, tricalcium aluminate — onto their surfaces, so hydration products precipitate there rather than wherever they happen to nucleate. Their surfaces also carry negative charge that pulls calcium, sodium and potassium ions into a tight local environment, feeding the reactions that build calcium silicate hydrate, the gel that is concrete's actual glue. The authors describe a three-stage sequence: nucleation early, faster hydration kinetics in the middle, pore refinement and densification of the aggregate-paste boundary at later ages.

The chemistry backs this up. Calcium hydroxide content in the control paste ran about 12%, and dropped in the 0.1% liquid mix while calcium carboaluminate hydrate peaks rose. That's consumption of calcium hydroxide in secondary reactions, not dilution. Elemental mapping showed calcium at 28.6 atomic percent in the treated sample versus 26.5 in the control, with less free carbon — the fingerprint of more complete hydration and less carbonation.

The full paper is open access through the American Chemical Society at doi.org/10.1021/acsomega.6c03084, and a free full-text version is deposited with Europe PMC.

Where the effect falls apart

Three things go wrong, and the paper doesn't hide any of them.

More is worse. The 0.3% liquid mix produced 33.9 MPa at 28 days in the 24 MPa class; the 0.05% powder produced 29.5 MPa; the 0.1% liquid produced 37.8 MPa. The authors' own conclusion: “an ideal dosage threshold exists, beyond which aggregation and inadequate dispersion outweigh any potential advantages.” Electron microscopy found needle-shaped precipitates in the higher-dose and powder mixes, consistent with delayed ettringite formation tied to carbonation — ettringite being a sulphate mineral whose late, expansive growth cracks concrete from the inside.

Powder loses to liquid. The dry form clumps in the mix and never distributes evenly, which is why its water absorption (5.0%) sat between the control and the liquid dose, and why its pore volume barely moved.

Acid resistance is the weakest claim in the paper, and the authors say so. “The enhancement was not consistently observed for all mixtures.” In the 42 MPa class after 28 days of acid immersion, the control retained 40.0 MPa and the 0.1% liquid mix retained 39.3 — a reversal. The 32 MPa class was a tie at 32.2 and 32.1. The gains are real where they appear: 28 MPa concrete went from 23.7 MPa to 30.3 MPa after 56 days in acid, and the best case showed up to 28% higher residual strength. But the effect is conditional on grade, dose and form, not a blanket improvement.

What the paper does not claim

The experiments ran in a laboratory, on one cement source, one aggregate source, and dots from a single supplier — CrystalLyte of Bangkok. Acid exposure stopped at 56 days. Real sewer walls and marine pilings see years of wetting and drying, chloride cycles and microbial activity that no immersion test reproduces. The authors name this themselves: future work should address long-term durability under real environmental conditions, plus how the dots interact with supplementary cementitious materials such as fly ash or slag, where the low-carbon case actually gets made.

Cost is the other open question, and it isn't addressed in this paper. A 2025 systematic review of carbon and graphene quantum dots in construction materials, led by co-author Lapyote Prasittisopin, put GQD pricing in the same range as polycarboxylate superplasticisers — thousands of baht per kilogram — while flagging the energy demand of synthesis as a live concern. At 0.1% dosing the additive is cheap per cubic metre of concrete. At 0.3% it stops being cheap, and that's exactly the dose where performance declined.

An independent materials researcher reading these results would note one more thing: three of the four strength classes gained 6–7% or less on compressive strength, and the 32% figure comes from the weakest mix. That is still a good outcome — low-grade concrete is where porosity is worst and where improvement is easiest — but a specification engineer needs to know the gain is grade-specific, not a uniform uplift.

Funding came from the Second Century Fund at Chulalongkorn University through a postdoctoral research fellowship. The authors credit CrystalLyte for supplying the graphene quantum dots. The paper carries a CC BY-NC-ND 4.0 licence and is deposited in Victoria University's institutional repository at vuir.vu.edu.au.

a black and white photo of a cell phone

Photo by TSD Studio on Unsplash

The next five years

The commercial path for a nanoadditive runs through batching plants, and batching plants don't buy chemistry, they buy slump and 28-day certificates. On slump, the dots behaved well: 5–10 mm more flow across all grades, up to 15 mm in the 42 MPa class at 0.3%, because the hydrophilic surfaces hold water that would otherwise be bound and because the dots help the superplasticiser separate cement grains. That's a selling point with no durability claim attached.

The harder problem is verification. A ready-mix supplier adding 0.1% of anything needs a quality-control test that confirms dispersion on the day, not a 43% mesopore reduction measured six months later in a nitrogen isotherm. Until there is a fast field proxy for how well the dots are dispersed, the dose window between 0.1% and 0.3% stays uncomfortably narrow for site work.

Where this could matter first is not glamorous infrastructure. It's the concrete that suffers most: wastewater collection systems, agricultural structures, coastal foundations, cooling towers — the assets eaten by acid and sulphate before their design life is out. Those are also the assets where raising the strength grade is expensive and where a 25% cut in water absorption changes the maintenance calendar.

Global cement emissions sat near 1.47 billion tonnes of CO₂ in 2024, according to Our World in Data, and the sector's net-zero roadmap leans on clinker substitution and carbon capture. Neither gets easier. A kilogram of quantum dots per tonne of cement is a small enough intervention to fit into an existing plant's admixture line without touching the kiln — which is precisely why the next round of studies, on real exposure sites and blended cements, is the one worth watching.

  • materials-science
  • sustainable-construction
  • civil-engineering-research
  • acs-omega
  • nanomaterials
Portrait of Jarrod Kanizay
About the author

Jarrod KanizayView author

Academic Jobs In House Author

Visionary leader transforming academic recruitment with 20+ years in higher education.

Acknowledgements:

Discussion

Sort by:

Be the first to comment on this article!

You

You’ll be asked to sign in before your comment is posted.

Browse by Faculty

Browse by Subject

Frequently Asked Questions

🔬What are graphene quantum dots and why put them in concrete?

Graphene quantum dots (GQDs) are fragments of graphene — a one-atom-thick sheet of carbon — small enough that their edges and surface chemistry dominate their behaviour, typically under 20 nanometres across. In cement they act as nucleation sites for hydration products and their oxygen-bearing surface groups attract clinker minerals and calcium ions. Win and colleagues found that 0.1% liquid GQDs by weight of cement raised 28-day compressive strength by up to 32% and cut mesopore volume by about 43%.

📊How much of a strength gain did the study measure?

At 28 days, the 24 MPa concrete rose from 28.6 MPa to 37.8 MPa with 0.1% liquid GQDs, a 32% increase. The 28 MPa class went from 32.1 to 40.7 MPa (27%). The 32 MPa class moved from 34.6 to 37.1 MPa and the 42 MPa class from 44.5 to 47.1 MPa — gains of roughly 6–7%. Splitting tensile strength increased by up to 36% and flexural strength by about 18%.

⚗️Why does the paper argue the dots are not just filler?

Because the chemistry moved. Thermogravimetric analysis showed calcium hydroxide content in the control paste at about 12%, dropping in the 0.1% liquid mix while calcium carboaluminate hydrate peaks rose in X-ray diffraction — evidence of secondary reactions consuming calcium hydroxide rather than dilution. BET analysis showed surface area falling from 16.82 to 9.54 m²/g and pore volume from 0.051 to 0.029 cm³/g. A purely physical filler would not redirect which hydrate phases form.

⚠️What happens if you add more graphene quantum dots?

Performance falls. In the 24 MPa class, 0.1% liquid GQDs delivered 37.8 MPa at 28 days, while 0.3% delivered 33.9 MPa. The authors conclude that an ideal dosage threshold exists beyond which aggregation and poor dispersion outweigh the benefits. Electron microscopy found needle-like precipitates in the higher-dose and powder mixes, consistent with delayed ettringite formation linked to carbonation.

💧Is liquid or powdered graphene quantum dots better?

Liquid, consistently. The powder form (GQDs-P at 0.05%) produced 29.5 MPa at 28 days in the 24 MPa class against 37.8 MPa for the liquid at 0.1%. It also reduced water absorption only to 5.0% against 4.5% for the liquid, and barely shifted pore volume. The authors attribute the gap to clumping: dry dots are harder to distribute evenly through the paste, and uneven distribution wastes the surface chemistry that does the work.

🧪Did the additive improve acid resistance?

Partly. After 56 days of acid immersion, 28 MPa concrete retained 30.3 MPa with 0.1% liquid GQDs against 23.7 MPa for the control, and the 42 MPa class went from 28.6 to 37.2 MPa. The best case showed up to 28% higher residual compressive strength. But the paper states that the enhancement was not consistently observed for all mixtures — in the 42 MPa class after 28 days of acid, the treated mix retained 39.3 MPa against the control's 40.0 MPa.

🕳️What does mesopore volume have to do with durability?

Mesopores are the voids between roughly 10 and 50 nanometres. They are the channels water, sulphate and chloride use to travel through hardened cement paste, and their connectivity controls permeability more than total porosity does. Cutting mesopore volume by about 43% means fewer connected pathways for aggressive ions. In the study, water absorption fell from 6.0% to 4.5% in the 24 MPa class and porosity from 15.9% to 10.8%.

💰Who funded this research and were there conflicts of interest?

The authors acknowledge the Second Century Fund (C2F) at Chulalongkorn University for a postdoctoral research fellowship, and thank CrystalLyte Co., Ltd. for supplying the graphene quantum dots used in the study. The paper is published open access in ACS Omega under a CC BY-NC-ND 4.0 licence and is deposited in Victoria University's institutional repository.

🔎What are the limitations of the study?

The tests were laboratory-scale, using one ordinary Portland cement source, one aggregate source and GQDs from a single supplier. Acid exposure ran to a maximum of 56 days of immersion, which does not reproduce years of wetting and drying, chloride cycling or microbial attack in real service. The authors call for future work on long-term durability under real environmental conditions and on how GQDs interact with supplementary cementitious materials for low-carbon concrete.

🌍Does this research reduce concrete's carbon footprint?

Not directly — cement emissions are unchanged by an additive dosed at 0.1%. The climate case is indirect: longer service life spreads the same embodied carbon across more years of use, and less maintenance means less repair concrete. The authors flag the interaction between GQDs and supplementary cementitious materials such as fly ash or slag as a priority for future work, since that is where the actual low-carbon formulation gains sit.

🎓Where is Thwe Thwe Win based and what else has she published?

Win is at the University of Lisbon and has spent several years on graphene-based nanoadditives in cementitious systems. Earlier work includes studies on graphene nanoplatelets in calcium aluminate cement, supra-GQDs for conductive cement composites published in Construction and Building Materials, and a 2024 paper in the Journal of Building Engineering on GQDs for thermal and mechanical performance, where 0.3% Qdl produced 20.8% and 50% increases in compressive and flexural strength respectively.

🏗️What applications would benefit most from this approach?

The likeliest early adopters are structures exposed to acid and sulphate — wastewater collection systems, agricultural buildings, coastal foundations, cooling towers — where concrete often fails well before its design life. Low-grade 24 MPa concrete showed the largest porosity and absorption reductions, and that grade is common in pavements, drainage works and low-rise frames. High-strength structural concrete gained far less, so the case there is weaker on current evidence.